EPA Method 312A Determination Of Styrene In Latex Styrene-Butadiene Rubber, Through Gas Chromatography

ID

068A9B3E11054AC4B000ACA260E1A612

文件大小(MB)

0.03

页数:

5

文件格式:

pdf

日期:

1998-5-13

购买:

购买或下载

文本摘录(文本识别可能有误,但文件阅览显示及打印正常,pdf文件可进行文字搜索定位):

1,METHOD 312A - DETERMINATION OF STYRENE IN LATEX STYRENE-BUTADIENE,RUBBER, THROUGH GAS CHROMATOGRAPHY,1. SCOPE AND APPLICATION,1.1 This method describes a procedure for determining parts,per million (ppm) styrene monomer (CAS No. 100-42-5) in,aqueous samples, including latex samples and styrene,stripper water.,1.2 The sample is separated in a gas chromatograph equipped,with a packed column and a flame ionization detector.,2.0 SUMMARY OF METHOD,2.1 This method utilizes a packed column gas chromatograph,with a flame ionization detector to determine the,concentration of residual styrene in styrene butadiene,rubber (SBR) latex samples.,3.0 DEFINITIONS,3.1 The definitions are included in the text as needed.,4.0 INTERFERENCES,4.1 In order to reduce matrix effects and emulsify the,styrene, similar styrene free latex is added to the,internal standard. There are no known interferences.,4.2 The operating parameters are selected to obtain,resolution necessary to determine styrene monomer,concentrations in latex.,5.0 SAFETY,5.1 It is the responsibility of the user of this procedure,to establish appropriate safety and health practices.,6.0 EQUIPMENT AND SUPPLIES,6.1 Adjustable bottle-top dispenser, set to deliver 3 ml.,(for internal standard), Brinkmann Dispensette, or,equivalent.,6.2 Pipettor, set to 10 ml., Oxford Macro-set, or,equivalent.,2,6.3 Volumetric flask, 100-ml, with stopper.,6.4 Hewlett Packard Model 5710A dual channel gas,chromatograph equipped with flame ionization detector.,6.4.1 11 ft. x 1/8 in. stainless steel column packed,with 10% TCEP on 100/120 mesh Chromosorb P, or,equivalent.,6.4.2 Perkin Elmer Model 023 strip chart recorder, or,equivalent.,6.5 Helium carrier gas, zero grade.,6.6 Liquid syringe, 25-μl.,6.7 Digital MicroVAX 3100 computer with VG Multichrom,software, or equivalent data handling system.,6.6 Wire Screens, circular, 70-mm, 80-mesh diamond weave.,6.7 DEHA - (N,N-Diethyl hydroxylamine), 97+% purity, CAS,No. 3710-84-7,6.8 p-Dioxane, CAS No. 123-91-1,7.0 REAGENTS AND STANDARDS,7.1 Internal standard preparation.,7.1.1 Pipette 5 ml p-dioxane into a 1000-ml volumetric flask and fill to,the mark with distilled water and mix thoroughly.,7.2 Calibration solution preparation.,7.2.1 Pipette 10 ml styrene-free latex (eg: NBR latex) into a 100-ml volumetric flask.,7.2.2 Add 3 ml internal standard (section 7.1.1 of this method).,7.2.3 Weigh exactly 10 μl fresh styrene and record the weight.,7.2.4 Inject the styrene into the flask and mix well.,7.2.5 Add 2 drops of DEHA, fill to the mark with water and mix well again.,7.2.6 Calculate concentration of the calibration solution as follows:,R’E(Rn)/6,Rn,’(cns,&c<)/Sn,3,mg/l styrene = (mg styrene added)/0.1 L,8.0 SAMPLE COLLECTION, PRESERVATION, AND STORAGE,8.1 A representative SBR emulsion sample should be caught in a clean, dry 6-oz.,teflon lined glass container. Close it properly to assure no sample leakage.,8.2 The container should be label with sample identification, date and time.,9.0 QUALITY CONTROL,9.1 The instrument is calibrated by injecting calibration solution (Section 7.2 of this,method) five times.,9.2 The retention time for components of interest and relative response of monomer to,the internal standard is determined.,9.3 Recovery efficiency must be determined once for each sample type and whenever,modifications are made to the method.,9.3.1 A set of six latex samples shall be collected. Two samples shall be prepared for,analysis from each sample. Each sample shall be analyzed in duplicate.,9.3.2 The second set of six latex samples shall be analyzed in duplicate before spiking,each sample with approximately 1000 ppm styrene. The spiked samples shall be,analyzed in duplicate.,9.3.3 For each hydrocarbon, calculate the average recovery efficiency (R) using the,following equations:,where:,where:,n = sample number,c = concentration of compound measured in spiked sample number n. ns,c = concentration of compound measured in unspiked sample number n. nu,S = theoretical concentration of compound spiked into sample n. n,4,9.3.4 A value of R between 0.70 and 1.30 is acceptable.,9.3.5 R is used to correct all reported results for each compound by dividing the,measured results of each compound by the R for that compound for the same,sample type.,10.0 CALIBRATION AND INSTRUMENT SETTINGS,10.1 Injection port temperature, 250EC.,10.2 Oven temperature, 110EC, isothermal.,10.3 Carrier gas flow, 25 cc/min.,10.4 Detector temperature, 250EC.,10.5 Range, 1X.,11.0 PROCEDURE,11.1 Turn on recorder and adjust baseline to zero.,11.2 Prepare sample.,11.2.1 For latex samples, add 3 ml Internal Standard (section 7.1 of this method) to a……

……